Tensile and torsional stress corrosion testing machine is mainly used to detect and study metal materials, metal products, etc., in the static permanent tensile/torsion, corrosion environment of the material corrosion tensile mechanical properties test and measure its thermal deformation characteristics.
Product Introduction:
Tensile and torsional stress corrosion testing machine is mainly used to detect and study metal materials, metal products, etc., in the static permanent tensile/torsion, corrosion environment of the material corrosion tensile mechanical properties test and measure its thermal deformation characteristics
Technical parameters:
1. Maximum test force: 20KN
2, test force range: 0.4%FS ~ 100%FS
3, test force value accuracy: ≤±1%
4, tensile test speed range: 10-6mm/min ~ 1mm/min stepless adjustment
5, drawing speed control accuracy: ≤±0.5%
6, stretching stroke: 0 ~ 200mm
7. Maximum torque: 50NM
8, torque value accuracy: ≤±1%
9, tensile test speed range: 1°/min ~ 120°/min stepless adjustment
10, speed indication accuracy: ≤±1
11, control mode: force, displacement, torque, speed loading; Touch screen and test software dual display dual control.
12, tensile deformation range: 0-10mm
13, reactor heating temperature: room temperature ~ 80℃
14, temperature accuracy: ≤±1℃
15, pressure: 0 ~ 20MPa
16, pressure accuracy: ≤0.1MPa