Products

  • Multi-axial tensile and torsional stress corrosion testing machine

Multi-axial tensile and torsional stress corrosion testing machine

Tensile and torsional stress corrosion testing machine is mainly used to detect and study metal materials, metal products, etc., in the static permanent tensile/torsion, corrosion environment of the material corrosion tensile mechanical properties test and measure its thermal deformation characteristics.

Introduction

Product Introduction:

       Tensile and torsional stress corrosion testing machine is mainly used to detect and study metal materials, metal products, etc., in the static permanent tensile/torsion, corrosion environment of the material corrosion tensile mechanical properties test and measure its thermal deformation characteristics



Parameters

Technical parameters:

1. Maximum test force: 20KN

2, test force range: 0.4%FS ~ 100%FS

3, test force value accuracy: ≤±1%

4, tensile test speed range: 10-6mm/min ~ 1mm/min stepless adjustment

5, drawing speed control accuracy: ≤±0.5%

6, stretching stroke: 0 ~ 200mm

7. Maximum torque: 50NM

8, torque value accuracy: ≤±1%

9, tensile test speed range: 1°/min ~ 120°/min stepless adjustment

10, speed indication accuracy: ≤±1

11, control mode: force, displacement, torque, speed loading; Touch screen and test software dual display dual control.

12, tensile deformation range: 0-10mm

13, reactor heating temperature: room temperature ~ 80℃

14, temperature accuracy: ≤±1℃

15, pressure: 0 ~ 20MPa

16, pressure accuracy: ≤0.1MPa                          