The slow strain rate stress corrosion testing machine is mainly used to test and study the mechanical properties of metal materials, metal products, etc. under static tensile stress, simulated corrosion conditions, temperature, force, etc., and measure their thermal deformation characteristics.
|
Parameter |
Specification |
|
Overall Accuracy Class |
0.5 |
|
Test Force Range |
0.4% ~ 100% of full scale (FS), without range switching |
|
Test Force Resolution |
1/500,000 FS |
|
Test Speed Range |
0.00001 ~ 100 mm/min |
|
Deformation Resolution |
0.0001 mm |
|
Deformation Range |
0 - 12 mm |
|
Extensometer Range |
0.2% ~ 100% FS |
|
Alignment |
≤ 8% |
|
Tensile Stroke |
0 ~ 100 mm |
|
Maximum Test Space |
460 mm |
|
Test Control Modes |
Constant strain rate, constant stress rate, creep, stress relaxation, stepped (multi-stage) and cyclic loading (triangle wave, trapezoid wave; frequency: 0~1 Hz) |
|
Control Accuracy (Constant Force / Constant Deformation Rate) |
≤ ± 0.5% |
|
Heating Temperature Range |
Room temperature ~ 80°C |
|
Heating Method |
Direct heating and stirring circulation inside the corrosion tank to ensure concentration and temperature uniformity. |
|
Temperature Control Accuracy |
± 0.5°C |