Products

  • WDML-100 Slow strain rate stress corrosion testing machine

WDML-100 Slow strain rate stress corrosion testing machine

The slow strain rate stress corrosion testing machine is mainly used to test and study the mechanical properties of metal materials, metal products, etc. under static tensile stress, simulated corrosion conditions, temperature, force, etc., and measure their thermal deformation characteristics.

Introduction

WDML-100 slow strain rate stress corrosion testing machine is mainly used to test and study the mechanical properties of metal materials, metal products, etc. under static tensile stress, simulated corrosion conditions, temperature, force, etc., and measure their thermal deformation characteristics. The equipment fully meets the GB/T 15970.7-2017 Corrosion Stress Corrosion Testing of Metals and Alloys Part 7: Slow Strain Rate Test standard. It can achieve constant displacement rate loading, constant load loading, and holding load loading tests.

Parameters

Parameter

Specification

Overall Accuracy Class

0.5

Test Force Range

0.4% ~ 100% of full scale (FS), without range switching

Test Force Resolution

1/500,000 FS

Test Speed Range

0.00001 ~ 100 mm/min

Deformation Resolution

0.0001 mm

Deformation Range

0 - 12 mm

Extensometer Range

0.2% ~ 100% FS

Alignment

≤ 8%

Tensile Stroke

0 ~ 100 mm

Maximum Test Space

460 mm

Test Control Modes

Constant strain rate, constant stress rate, creep, stress relaxation, stepped (multi-stage) and cyclic loading (triangle wave, trapezoid wave; frequency: 0~1 Hz)

Control Accuracy (Constant Force / Constant Deformation Rate)

≤ ± 0.5%

Heating Temperature Range

Room temperature ~ 80°C

Heating Method

Direct heating and stirring circulation inside the corrosion tank to ensure concentration and temperature uniformity.

Temperature Control Accuracy

± 0.5°C

  • *Name
  • *Telephone
  • *Email
  • *Region
  • *Contact